Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® Advanced T1000HG6 LS BK - PA6T/6I-GF30 - BASF

Material Data Center offers the following functions for Ultramid® Advanced T1000HG6 LS BK:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Texto del producto
Heat stabilized, partially aromatic polyphthalamide for injection molding with strong mechanical properties especially at elevated temperatures and excellent chemical resistance for highly stressed parts. Ultramid® Advanced T1000HG6 LS BK can be characterized as compound with high strength and stiffness, very low water absorption and outstanding dimensional stability. It features a high melting point (320°C) and excellent melt stability.

Markets & applications
Automotive: Fuel system, cooling system, powertrain, Auto E&E, sensors, pumps, fuel cell
Industry goods: Pumps, compressors
Consumer goods: Home appliances, consumer electronics
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Contracción posterior al moldeo, paralelo 0.4 / * % ISO 294-4, 2577
Contracción posterior al moldeo, normal 1.0 / * % ISO 294-4, 2577
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 11800 / 12000 MPa ISO 527
Resistencia a la tracción 190 / 180 MPa ISO 527
Alargamiento a rotura 1.9 / 1.7 % ISO 527
Resistencia al impacto Charpy, +23°C 55 / 50 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 50 / 50 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 7.5 / 6.5 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 7 / 6.5 kJ/m² ISO 179/1eA
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 320 / * °C ISO 11357-1/-3
Temp. de transición vítrea, 10°C/min 130 / * °C ISO 11357-1/-2
Estabilidad al calor, 1.80 MPa 275 / * °C ISO 75-1/-2
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Resistividad superficial específica * / >1E15 Ohm IEC 62631-3-2
Resistencia dieléctrica 39 / - kV/mm IEC 60243-1
Indice comparativo de linea de fuga - / 600 - IEC 60112
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 4.1 / * % Sim. to ISO 62
Absorción de humedad 1.8 / * % Sim. to ISO 62
Densidad 1440 / - kg/m³ ISO 1183
Propiedades específicas del materialSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 105 / * cm³/g ISO 307, 1157, 1628
Condiciones de transformaciónValorUnidadesMétodo de ensayo
ISO Data
Moldeo por inyección, temperatura de la masa 350 °C ISO 294
Moldeo por inyección, temperatura del molde 150 °C ISO 294
Funciones
Módulo de cizallamiento dinámico-temperatura , Ultramid® Advanced T1000HG6 LS BK (Seco), PA6T/6I-GF30, BASF
Módulo de cizallamiento dinámico-temperatura , Ultramid® Advanced T1000HG6 LS BK (Cond), PA6T/6I-GF30, BASF
Esfuerzo-alargamiento , Ultramid® Advanced T1000HG6 LS BK (Seco), PA6T/6I-GF30, BASF
Esfuerzo-alargamiento , Ultramid® Advanced T1000HG6 LS BK (Cond), PA6T/6I-GF30, BASF
Módulo secante-alargamiento , Ultramid® Advanced T1000HG6 LS BK (Seco), PA6T/6I-GF30, BASF
Módulo secante-alargamiento , Ultramid® Advanced T1000HG6 LS BK (Cond), PA6T/6I-GF30, BASF
Módulo a tensión-temperatura , Ultramid® Advanced T1000HG6 LS BK (Seco), PA6T/6I-GF30, BASF
Módulo a tensión-temperatura , Ultramid® Advanced T1000HG6 LS BK (Cond), PA6T/6I-GF30, BASF
Características
Procesamiento y forma de entrega
Moldeo por inyección
Forma de suministro
Sémola, Negro
Características especiales
Estable contra el calor
Características
Resistencia del fundido
Resistencia quimica
Resistencia química general
Applicaciones
Automotriz, Electrica
Disponibilidad regional
Demás información
Moldeo por inyección
PREPROCESSING
Pre/Post-processing, max. allowed water content: .05 %
Pre/Post-processing, Pre-drying, Temperature: 120 °C
Pre/Post-processing, Pre-drying, Time: 8 h

PROCESSING
injection molding, Melt temperature, range: 335 - 355 °C
injection molding, Melt temperature, recommended: 350 °C
injection molding, Mold temperature, range: 140 - 170 °C
injection molding, Mold temperature, recommended: 150 °C
injection molding, Dwell time, thermoplastics: 5 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.